Home/Store/Plastics/ISO Test Methods/Thermal Properties (ISO)
760-2027-4 Differential Scanning Calorimetry (DSC) of Thermoplastics

760-2027-4 Differential Scanning Calorimetry (DSC) of Thermoplastics

$404.00
Closes 15 Nov
Ship To
Please choose
In stock
1
Save this product for later

760-2027-4 Differential Scanning Calorimetry (DSC) of Thermoplastics

Product Details

Enrollment Deadline: 15 November 2026

Participants will test samples using ISO 11357 and a heating rate of 20°C/minute. Two samples are used to test crystallization temperature (Tc), melt temperature (Tm), enthalpy of fusion (Hm), and enthalpy of crystallization (Hc), and two samples are used to test glass transition temperature (Tg). Laboratories may report any or all of the offered properties, including optional research properties for ASTM D3418.

Sample Description: Four sealed moisture barrier bags, each containing 10 g of polymer, which may come from the same batch or different batches. Enough material is supplied for labs to perform at least three test runs.

Samples ship in January, April, July, and October for a total of four shipments.

ISO Test Method 11357 is included on CTS' Scope of Accreditation to ISO/IEC 17043. ASTM D3418 is pending inclusion on CTS' Scope of Accreditation to ISO/IEC 17043.

Show More
  • My Account
  • Track Orders
  • Favorites
  • Shopping Bag
Powered by Lightspeed
Display prices in:USD
Skip to main content
CTS Online Store
Menu
Store
Industry Home
Forensics Home
571-434-1925info@cts-interlab.com
©Collaborative Testing Services P.O. Box 650820, Sterling VA, USA 20165-0820 1-571-434-1925
Report Abuse
Powered by Lightspeed